Sika® Injection-190 GB
MICRO CEMENT INJECTION GROUT
2-part, sustainable mineral injection grout based on microcement binders with added corrosion inhibitors (d95 < 9.5 μm).
- Structural grouting of cracks
- Corrosion protection of embedded reinforcement
- Deep penetration of narrow cracks in concrete and mortar
- Good flow properties
- Sustainable injeciton grout
Usage
- Injection of SikaFuko® injection hoses (VT-1 & VT-2)
- Filling of voids
- Final, rigid, cementitious sealing of cracks while simultaneously treating corroding or corrosion-prone reinforcing steel in concrete and mortar
Advantages
- Structural grouting of cracks
- Corrosion protection of embedded reinforcement
- Deep penetration of narrow cracks in concrete and mortar
- Good flow properties
- Sustainable injeciton grout
Packaging
Part A: | 20 kg bag | Powder component |
Part B: | 13 kg container | Liquid component |
Part A + B: | 33 kg | Ready mix unit |
Product Details
Chemical Base
Modified micro cement and supplementary cementitious material
Shelf Life
In unopened original packaging: 12 months from date of production
Storage Conditions
The product must be stored in original, unopened and undamaged sealed packaging in dry conditions at temperatures between +5 °C and +30 °C. Always refer to packaging.
Density
Part A + B: ~ 1.70 kg/l (+20 °C)
Viscosity
~ 450 mPa·s (+20 °C @ 12 RPM, Spindle No.63)
Compressive Strength
1 day: | ~ 7 MPa |
28 days: | ~ 50 MPa |
Application
Ambient Air Temperature
Min. +5 °C, max. +35 °C
Mixing Ratio
Part A : B: 1 : 0.65 (by weight)
Substrate Temperature
Min. +5 °C, max. +35 °C
Pot Life
~ 1 hour
Keep in movement when not in use. (Extended mixing may increase initial set time)
Yield
Pre-batched unit of 33 kg gives: ~20 L of injection grout
APPLICATION INSTRUCTIONS
SUBSTRATE PREPARATION
The substrate must be sound, clean, free of oil and grease, old coatings and other contaminations.
For good adhesion, pre-treat the substrate with high pressure water or mechanically.
Use air pressure to remove dust from cracks.
MIXING
Place the liquid part B in a suitable mixing vessel. Mix with colloidal mixer at a minimum 2 800 rpm and add the powder part A slowly and continuously. Mix the suspension thoroughly for at least 5 minutes.
Subsequently, pour the injection material directly into the pump or keep ready in a clean container.
APPLICATION METHOD / TOOLS
The injection material can be injected with commercially available equipment designed for cement injections (injection pressure 3 - 8 bar).
Start injecting at low pressure and build as necessary.
For vertical injection sections, inject from bottom to top.
If dry concrete has to be injected, it is recommended to pre-wet the concrete with water under light pressure.
In order to enable post-injections, the freshly injected section of the SikaFuko® systems (or the injection packers) must be thoroughly rinsed.
CLEANING OF TOOLS
Clean tools with water immediately after use.
Hardened material can only be removed mechanically.